Owing to their brittleness and heterogeneity, achieving carbon fiber-reinforced silicon carbide ceramic (Cf/SiC) composites with ideal dimensional and shape accuracy is difficult. In this study, unidirectional Cf materials were subjected to orthogonal grinding experiments using different fiber orientations. Through a combined analysis of the surface morphology and grinding force after processing, the mechanism underlying the effect of the fiber orientation on the surface morphology of the material was explained. The surface roughness of the material was less affected by the process parameters and fluctuated around the fiber radius scale; the average surface roughness (Ra) in the direction of scratching parallel (SA) and perpendicular (SB) to the fiber direction was 4.21-5.00 μm and 4.42-5.26 μm, respectively; the material was mainly removed via the brittle removal mechanism; and the main defects of the fiber in the SA direction were tensile fracture and extrusion fracture; the main defects of the fiber in the SB direction were bending fracture, shear fracture, and fiber debonding. The grinding parameters influenced the grinding force in the order: depth of cut > feed rate > wheel speed. The grinding force increased with an increase in the feed rate or depth of cut and decreased with an increase in the wheel speed. Moreover, increasing the depth of cut was more effective in decreasing the grinding force and improving the material removal efficiency than adjusting the rotational speed of the workpiece and the rotational speed of the grinding wheel. The specific grinding energy decreased with an increase in the feed rate or depth of cut, and increased with an increase in the grinding wheel speed.
The full text can be downloaded at https://link.springer.com/article/10.1007/s40436-024-00521-0
Chong-Jun Wu
,
Fei Liu
,
Jia-Zhou Wen
,
Pei-Yun Xia
,
Steven Y. Liang
. Grinding defect characteristics and removal mechanism of unidirectional Cf/SiC composites[J]. Advances in Manufacturing, 2025
, 13(1)
: 211
-228
.
DOI: 10.1007/s40436-024-00521-0
[1] Diao QW, Zou HB, Ren XY et al (2023) A focused review on the tribological behavior of C/SiC composites: present status and future prospects. J Eur Ceram Soc 43(9):3875-3904
[2] Dong Z, Yan Y, Peng G et al (2023) Effects of sandwiched film thickness and cutting tool water contact angle on the processing outcomes in nanoskiving of nanowires. Mater Des 225:111438. https://doi.org/10.1016/j.matdes.2022.111438
[3] Arai Y, Inoue R, Goto K et al (2019) Carbon fiber reinforced ultra-high temperature ceramic matrix composites: a review. Ceram Int 45(12):14481-14489
[4] Kong JH, Lee SY, Son YI et al (2023) Synergistic reinforcement effects of ZrB2 on the ultra-high temperature stability of Cf/SiC composite fabricated by liquid silicon infiltration. J Eur Ceram Soc 43(8):3062-3069
[5] Lou ZZ, Yan YD, Wang JQ et al (2024) Exploring the structural color of micro-nano composite gratings with FDTD simulation and experimental validation. Opt Express 32(2):2432-2451
[6] Piao YC, Li C, Hu YX et al (2024) Nanoindentation induced anisotropy of deformation and damage behaviors of MgF2 crystals. J Mater Res Technol 28:4615-4625
[7] Wang JQ, Yan YD, Li C et al (2023) Material removal mechanism and subsurface characteristics of silicon 3D nanomilling. Int J Mech Sci 242:108020. https://doi.org/10.1016/j.ijmecsci.2022.108020
[8] Zahabi S, Arjmand H, Ramazani M et al (2023) The effect of alumina-based sintering aid on the microstructure, selected mechanical properties, and coefficient of friction of Cf/SiC composite prepared via spark plasma sintering (SPS) method. Ceram Int 49(10):15253-15265
[9] Feoktistov D, Kuznetsov G, Sivkov A et al (2022) Expanding the scope of SiC ceramics through its surface modification by different methods. Surf Coat Technol 435:128263. https://doi.org/10.1016/j.surfcoat.2022.128263
[10] Sarabjit S, Vajinder S, Sweety K et al (2019) A comparative study of tensile strength of Cf/SiC composites having single layer and multilayer interphases. Ceram Int 45(17):21193-21199
[11] Mubina S, Khanra A, Saha B (2020) Enhancement of oxidation resistance of CVD SiC coated Cf/C-SiC hybrid composite tubes processed through Si-infiltration. J Alloys Compd 826:154107. https://doi.org/10.1016/j.jallcom.2020.154107
[12] Wu CJ, Li BZ, Liu Y et al (2017) Surface roughness modeling for grinding of silicon carbide ceramics considering co-existence of brittleness and ductility. Int J Mech Sci 133:167-177
[13] Diaz OG, Luna GG, Liao Z et al (2019) The new challenges of machining ceramic matrix composites (CMCs): review of surface integrity. Int J Mach Tools Manuf 139:24-36
[14] Li C, Hu YX, Wei ZZ et al (2024) Damage evolution and removal behaviors of GaN crystals involved in double-grits grinding. Int J Extreme Manuf 6(2):025103. https://doi.org/10.1088/2631-7990/ad207f
[15] Wu CJ, Zhang TY, Guo WC et al (2022) Laser-assisted grinding of silicon nitride ceramics: micro-groove preparation and removal mechanism. Ceram Int 48(21):32366-32379
[16] Wan YH, Song XB, Zhao GL et al (2023) Design of discrete-edge polycrystalline diamond tool and its cutting performance in milling Cf/SiC composites. Diam Relat Mater 137:110153. https://doi.org/10.1016/j.diamond.2023.110153
[17] Rampal KG, Rangappa S et al (2022) A review of recent advancements in drilling of fiber-reinforced polymer composites. Compos Part C: Open Access 9:100312. https://doi.org/10.1016/j.jcomc.2022.100312
[18] Cao C, Song QH, Fu H et al (2023) Fiber orientation effects on grinding characteristics and removal mechanism of 2.5D Cf/SiC composites. Chin J Aeronaut 36(12):1000-9361
[19] Du JG, Ming WY, Ma J et al (2018) New observations of the fiber orientations effect on machinability in grinding of C/SiC ceramic matrix composite. Ceram Int 44(12):13916-13928
[20] Qu SS, Yao P, Gong YD et al (2022) Modelling and grinding characteristics of unidirectional C-SiCs. Ceram Int 48(6):8314-8324
[21] Zhang L, Wang S, Li Z et al (2019) Influence factors on grinding force in surface grinding of unidirectional C/SiC composites. Appl Compos Mater 26(3):1073-1085
[22] Li YC, Ge X, Wang H et al (2019) Study of material removal mechanisms in grinding of C/SiC composites via single-abrasive scratch tests. Ceram Int 45(4):4729-4738
[23] Pang JW, Li S, Guo MB et al (2023) Drilling of C/SiC composite micro holes with electroplated diamond bits. Diamond Abras Eng 43(1):90-95
[24] Wu Z, Zhang L, Yang S et al (2022) Effects of grain size and protrusion height on the surface integrity generation in the nanogrinding of 6H-SiC. Tribol Int 171:107563. https://doi.org/10.1016/j.triboint.2022.107563
[25] Wu ZH, Zhang LC, Yang SY (2021) Effect of abrasive grain position patterns on the deformation of 6H-silicon carbide subjected to nano-grinding. Int J Mech Sci 211:106779. https://doi.org/10.1016/j.ijmecsci.2021.106779
[26] Azizi A (2015) Modeling and analysis of grinding forces based on the single grit scratch. Int J Adv Manuf Technol 8:1223-1231
[27] Zhang X, Kang Z, Li S et al (2019) Grinding force modelling for ductile-brittle transition in laser macro-microstructured grinding of zirconia ceramics. Ceram Int 45:18481-18500
[28] Song Y, Cao HJ, Zheng W et al (2022) Cutting force modeling of machining carbon fiber reinforced polymer (CFRP) composites: a review. Compos Struct 299:116096. https://doi.org/10.1016/j.compstruct.2022.116096
[29] Gao H, Li RQ, Xu QH et al (2023) Feasibility study on SiO2f/SiO2 composites processed by diamond tools. Diamond Abras Eng 43(1):75-81
[30] Zhou K, Xiao GJ, Huang Y (2022) Understanding machinability improvements and removal mechanism of ceramic matrix composites during laser-ablating assisted grinding. Wear 538/539:205199. https://doi.org/10.1016/j.wear.2023.205199
[31] Hua H, Li JX, Zhu ZY et al (2023) A review of mixed mode I-II fracture criteria and their applications in brittle or quasi-brittle fracture analysis. Theor Appl Fract Mech 124:103741. https://doi.org/10.1016/j.tafmec.2022.103741
[32] Xiao GJ, Li X, Zhou K et al (2023) Comprehensive investigation into grinding characteristics and damage behavior of Cf/SiC composite modified by picosecond-laser ablating. Compos Struct 325:117600. https://doi.org/10.1016/j.compstruct.2023.117600
[33] Diaz O, Axinte D, Smith P et al (2019) On understanding the microstructure of SiC/SiC ceramic matrix composites (CMCs) after a material removal process. Mater Sci Eng: A 743:1-11
[34] Qu SS, Yao P, Gong YD et al (2022) Environmentally friendly grinding of C/SiCs using carbon nanofluid minimum quantity lubrication technology. J Clean Prod 366:132898. https://doi.org/10.1016/j.jclepro.2022.132898
[35] Zhang ZK, Yuan SM, Xu WW et al (2022) Damage behavior and removal mechanism of different yarn orientations 2.5D SiCf/SiC composites under single-abrasive scratch test. Ceram Int 48(20):30868-30883
[36] Liu Q, Huang G, Xu X et al (2017) A study on the surface grinding of 2D C/SiC composites. Int J Adv Manuf Technol 93:1595-1603